Open Access

Table 4

Estimated yield strength and principal sources of hardening for the various microstructures.

  σYS(MPa) Martensitic transformation Precipitation SS effect
(% C mainly)
CX13 B 727   X (nano) X
CX13 M bulk 1205 X   X
CX13 M surface 1825 X X (micro) X
Ref. + Bulk treat. + Surf. Hard. 727+478+620      
XD15 F 603   X (micro)  
XD15 M bulk 989 X X (micro) X
XD15 M surface 1799 X X(micro) X
Ref. + Bulk treat. + Surf. Hard. 603+386+810      
MLX17 M bulk 1493 X X (nano)  
MLX17 M surface 1493 X X (nano)  